Menu

Making a Custom Glaze Drip Catcher for a Fjillip Medallion

I recently purchased the rights to a cute relief sculpted medallion of an adorable pony called "Fjillip" sculpted by my good friend, Rayvin Maddock of Khrysalis Studios.  She has already produced this piece in a limited 40 piece edition in resin up in Canada, but I got his unlimited rights to produce him in ceramics.  Here is an example of one of my porcelain casts of this lying down pony in porcelain and glazed by myself to a bay appaloosa.  Once fired to cone 6 he measures about 6 inches wide.  The piece may be displayed standing upright as shown, or laying down, or mounted on the wall, or framed, etc.



While I very often glaze these using low fire underglazes and overglazes to produce ultra realistic horse coat colors like the appaloosa above, I also like to 'art glaze' some to mid fire cone 5/6 colors that are unrealistic horse colors but are lovely all the same.  I especially like these art glazed pieces because they are much faster for me to produce, I can sell them for less, and I can use them as gifts and show awards!   With unlimited casting rights in ceramic I made a concept plaster mold to work with first, and soon I'll produce a very crisp rubber master from the resin copy I have that will allow me to quickly & easily pour as many ready to use plaster molds for slip casting as I could ever want.  That way I can produce hundreds of castings over time for years to come with ease and not have to tediously rebuild the mold making from scratch every time I need a new plaster mold of Fjillip.

 

For drippy, runny cone 5/6 glazes however, I also need glaze drip catchers!  If I don't have them my glazes can run off onto my kiln shelves, possibly ruining them and damaging the medallions when I try to chip them free!  Complex thin jewelry pendants or an oddly shaped relief sculpted pieces like this I could use balls of alumina wadding but it is too easy for the porcelain to warp and deform, or the glaze to run underneath and require a LOT of grinding to get the drips off.  So I decided to make a custom glaze catcher made to fit Fjillip precisely as I can. I may still have some glaze seep between that will need grinding off later, but hopefully not a lot.  Therefor I had to start blocking it in with oil clay to make a plaster waste mold from. 


This photo shows several jewelry cabochons I was forming for mold making that would allow me to do crystalline glaze testing on 'test tiles' that I could then utilize for making jewelry.  I can also attach them upright for vertical tests to a simple base as desired or use them flat, horizontally.  In the upper left you can see the resin casting of the Fjillip medallion I have already used to make a plaster slip casting mold from.  Here I am building up oil clay walls all the way around and am checking the fit of the resin within it.  Underneath the resin casting is a raised lower wall to act as the lip inside of the drip catcher.  Once I remove the resin cast I'm all ready to pour the plaster waste mold which I can then clean up and fine tune for the next steps.  In the case of the cabochons they can be first line production molds for casting porcelain.  I'll keep some castings as backups for making rubber master molds from later.

For the Fjillip, which I'd like a fairly precise fit for the glaze catcher, I propped the cleaned up flat plaster waste mold piece into a plastic container only slightly larger than it.  I positioned it so there was a gap all the way around and underneath so that the plaster, face down, could be slip cast in porcelain to produce a single cast.  Once carefully removed and trimmed up, you can see the fresh porcelain casting here, just below the waste plaster.


 

Now this single porcelain cast gets cleaned up.  Some of the walls are too thin and I'll need to thicken them to be consistent all the way around or they will too easily sag and collapse when fired. 


If I found that a fresh damp greenware casting were not practical to make a new plaster mold from, I could have pressed a slab of oil clay over the plaster, or oil soap the plaster and do the same with a slab of epoxy sheet of the thickness I desire.  Once it any of those materials are set enough, I can remove them carefully and reshape them until it is just right for casting a two part plaster mold.  If you prefer modling in 3D programs you can print out any of these components to make your molds from, whichever works best for you.



I've also cast a fresh porcelain of the Fjillip pony medallion.  Here, after a quick rough cleaning (I'll fine tune cleaning it up later) I can now carefully set it onto the glaze catcher casting to check the fit.  I won't bother to fine tune the fit too much right now other than needing to test it.  Is the lip high enough?  This piece being mostly horizontal rather than large and vertical, the height of the lip is probably sufficient - but I will cast a couple of these and adjust various lip heights to be sure I have one optimized for the glazes I intend to use.  It may also inform my choices on how best to make my plaster production mold for slip casting the drip trays.


Once I test fire using a few of these and have finalized my best design, a pour spout needs to be attached before I make that plaster mold so I'll be able to slip cast these drip trays for Fjillip as needed.  Or I can cut the pour spout out of the wet, soft plaster once I have poured it.  Using the half mold I have now does work but it's clunky and does not work as well as I need it to if I want to cast quite a few of these trays.


Whichever tray version I finally settle upon to use,  I don't want that casting to dry up too much before I make the plaster.   Or produce one in another material that matches the design specs I require.  I need to check it with a very soft, still wet casting of Fjillip as well so there isn't too much shrinkage on him either.  When fired I need them to match up carefully and shrink at the same rate together.  To do that I can spray both with a little water and put them into a damp box to rest until I'm all ready to pour the plaster.  I'll need to go find a suitable plastic container or build up oil clay of the right shape and size to form the containment for the plaster.


But before I do that I'll cast a few more drip trays, adjust the heights on the lips that hold up the medallion, and test fire them to decide what height is best on my final I will use to produce my mold. 


 

The new kiln cookies worked just fine.  However, after several test firings I found that I didn't need the raised lips at all.  The Fjillip medallions are flat enough, and low enough volume, that I have very little or no glaze running off and dripping onto the glaze catchers at all.  The only exception was one medallion that didn't come out right that I had to reglaze with three more layers - giving it a total of six layers of glaze at cone 6.  /That/ one did drip a little but still not much and was easy and fast to clean up.  


What does this mean?  I have no need of a raised lip on these kiln cookies.  So I don't need to refine and mold the custom glaze catchers at all.  I'll use them until they crack, then replace them with flat slab cookies as usual with no need for the porcelain pieces to be raised up from any pooling glaze that spills off - because it doesn't.  On a more vertical mug, bowl, or vase it would but for my purposes, testing proves that I can get by without going to the trouble.

 

I'll leave this blog post up because it is still useful for anyone in the future who has a problem with oddly shaped pieces in need of custom glaze drip catchers of unusual shape.  One sees that there can be a lot of useful testing with ceramics and not just for glaze combinations!  Thank you for reading on my adventures in firing ceramics.  ;)

 

 

 

Customizing a Hagen Renaker Daisy

Years ago I was given a very badly mutilated Hagen Renaker 'Daisy' sculpted by Maureen Love.  I think this Mustang mare may have been OF buckskin originally so this truly made me sad.  Some one (not me) tried to sandblast her original finish off to take her back to unglazed bisque.  Well, that sort of worked in a technical sense in that it did remove most of her glazed finish, but it also stripped off her sculpted detail, left a reptile like texture, and holes in her neck.  She still had two glued broken legs and was missing her front leg.  By the time she arrived to me, she was in horrible shape.  I was frankly quite at a loss what to do with her!

Recently I got this piece back out to give her some thought.  First I needed to remove the old glue from her two broken legs by firing her clean.  Then I needed to get rid of her reptile like texture and fill in the holes in her neck.  To do that I roughed up her body texture even more and coated her all over with bisque mender and then clay in a thin layer.  This further obliterated her details but she was already so messed up I figured I would have to resculpt everything back in later.

Here is the same bisque  now coated with clay to smooth out her strange texture.   She is ready for me to use diamond coated tools to deeply score the breaks in prep to reattach her legs using bisque mender.  I forgot to take a photo of her legs at that point so I'll insert a photo of a broken bisque Okie Rio's legs that I also scored at the same time so you can see how I have done it.   The deeper the scoring, the toothier the texture, the better!

This gives a nice roughed up surface to interlock with the newly added clay to reattach the legs.  For the missing leg on both bisques I also drilled out a hole and added a kiln rod to sculpt the missing leg back into place.  I could just sculpt & slip stick it on but adding the rod makes it harder for me to accidentally knock it off while I'm working!  The unfired legs when attached are very fragile and easy to break while cleaning up.

One way around that is to stand your piece up on a card.  I initially attach the legs to the piece with her flipped upside down as this is easiest to make sure the legs are straight before they can bear weight.  A hair dryer helps the clay to firm up quickly.  Once she is standing on cardstock it allows me to make certain all of her legs are the right length and her hooves flat.  It also makes it easier for me to do the rough clean up to shave off excess damp clay with a knife /without/ knocking the fragile leg repairs off.  Once dry I flipped her over and peeled off the card so I could finish initial cleanup.  As I can continue to do refinements after firing there is no need to get too nit picky the the details at this stage.

Now she is back on her feet and able to stand on her own!  Mind you that the repairs are not yet fired so she's fragile.  Handle with care.  I decided to go ahead and start resculpting her mane and tail as you can see here.  These areas are scored and bisque mender applied, then clay added.  The bisque mender with it's added flux & gum Arabic helps act like glue for a firmer bond to the bisque.

After adding more to the mane & tail, as well as her ears, I began to carve detail and coat texture back into her body using normal sculpting and dental tools.  Remember to work the clay damp if possible using a spritz of water to keep down dust.  Clay dust is very bad for your lungs so wear an appropriate mask or respirator rated for silca.  I also like to do any sanding over a dampened towel to catch dust as it falls from my piece.  I resculpted & refined this girl about as far as I dared while her legs are so easy to rebreak.  I did in fact knock off her repaired back leg THREE times while I was working on her.  Just be patient & reattach it however many times it takes.  I set her aside to dry by this point as I decided I wanted to bisque fire her repairs before I continued working.

And here she is after bisque firing in my kiln to Orton cone 04 (1945 degrees F).  Tada!  She now has four legs firmly attached.  There are some thin cracks to fill in with watered down bisque mender.  This piece is now ready for me to continue sculpting.  To build back her knees and add more to her tail I have to go back & deeply score the bisque all over again using diamond coated rotary cutting discs.  I will continue to refine and detail her legs, hooves, face and so forth until I have pushed her as far as I can.  When ready, I'll bisque fire her in the kiln at least once more before she will be ready for custom glazing to the color of my choice.  Probably an overo pinto!

Thank you for joining me for this blog segment.  I will make a new post in the future so you can see how this trashed Hagen Renaker Daisy gets a second chance to be appreciated when finished.


 


Customizing Already Glazed Ceramics

I started this particular topic in my previous blog post on 'Kiln Repairing Glazed Ceramics' so this is Part 2, continuation of the kiln repair of a Hagen Renaker 'Sherif' Arabian foal.  In this post I will talk about after the kiln repair of the already glazed piece.  If all I were doing to this earthenware foal was repairing it, I'd simply add white underglaze to match the body with a little grey shading, fire that, then clear glaze so that the entire body had the same sheen.  Tada!  All finished!  But as refiring any piece in the kiln will render it no longer truly 'original finish' then we may as well save OF pieces for cold repair techniques, and instead use kiln repairs to set up a piece for customizing.

After firing the leg repairs I wanted to push forward to also reshape the hooves to have nice, sharper edges, sand the bottom of the feet so the piece stands perfectly without any hint of wobble, resculpt the missing ear so it's flipped backwards, and redo the mane & tail to have more style!  This is the same 'Sherif' fired to repair the legs but without any glaze yet added to the bisque repairs.

Here is the other side showing her or his missing ear reculpted and flipped back.  I have used the same techniques to score the base of the ear deeply with toothy cuts so the new clay can grip & interlock with the already fired ceramic.  Then I also did the same to the mane and tail.  Already glazed, I simply cut deep toothy scoring into the mane & tail or I could have removed them entirely to add new replacements with or without using Kanthal rod to help me shape the tail.  Again I used bisque mender only here but I could have applied it initially for it's greater strength as dried greenware and then added regular earthenware clay right over it.

 

Here is a top view to show the mane and tail resculpting in progress before firing.  DO remember to wear protective mask suited to working with silica clay if you are at any point sanding or shaping DRIED clay or bisque mender.  Otherwise always work it while it's still damp or wet so there is no clay dust.  Here you can see I have added & detailed the mane but not yet detailed the tail in this shot.  If it cracks when drying, simply fill in any cracks as you go because the clay will shrink.  After bisque firing it, more cracks may appear as the clay shrank again while fired.  Fill those cracks in as well then you are ready to proceed either onto over glazes, or clear glazing.

Contrary to popular belief, YES you can add underglazes right over top of an already glazed piece!  If the glaze is also low fire then the underglaze will simply sink right into the glaze when you bisque fire it to cone 04 to mature the underglaze.  Work it as normal to lift, etch & otherwise prep each layer.  Fire as if it were a regular earthenware bisque.  As long as the underglaze you are adding isn't super thick it'll be fine & sink into the glaze layer below it.  If you apply the underglaze TOO thickly then it may form a crust that cracks rather than sinks into the glaze.  If that happens you can also repair it but better to not add too super thick a layer in the first place. 

Now we have the same Hagen Renaker 'Sherif' foal with the first layer of underglaze fired!  At this point the leg & ear repair are pretty hidden.  I continued on with the next layer of underglaze to detail the mane with hand painting.  Push everything as far as you need to in steps, add all the details you want, then bisque fire one more time.  After that you are ready to add your clear glaze and do what may be your final firing to cone 06 as normal, just the same as if this piece had been a bisque & not already glazed.

Tada!  This is the completed kiln repaired, resculpted & reglazed Hagen Renaker 'Sherif' Arabian foal to a soft baby 'black'.  Black foals are often grey or get sunburnt brown before they shed out their baby coat for a true black adult coat.  My client was thrilled with this piece and I am too.  Alternatively, if you overglaze, I could easily then continue working to custom glaze this piece to push it further.  Or if you don't work with underglazes, skip that stage to move right into clear glazing and then overglazing.  The actual kiln repairs can show however if you don't cover them with opaque colors so keep that in mind to build up layers or use specifically opaque rather than transparent over glazes such as opaque enamels before you progress to transparent china paints.  Have fun with it!

Watch out for future posts on how I actually resculpt a bisque or glazed piece to add a new mane & tail from start to finish.

Kiln Repairing Already Glazed Ceramics

I posted a step by step on how I kiln repair damaged bisques using a Dante as my example.  His legs being too thin to use Kanthal rods, or if your porcelain or fine bone china proves too difficult to drill out.  But what if the piece you want to kiln repair or resculpt is an already glazed piece such as a damaged Hagen Renaker?  Is it even possible?  Why yes!  It doesn't matter that it is already glazed, porcelain, earthenware or fine bone china - you handle it just the same as if it were a bisque.  That may sound risky, but pieces I have done using these techniques decades ago are still in perfect condition.  What better than the test of time?

Back in 2022 a client sent me a Hagen Renaker 'Sherif' Arabian foal with two broken legs and a broken ear.  It was already glazed a light grey-white in it's original finish.  This client had seen me resculpting & reglazing other already glazed pieces for decades.  She challenged me to repair and resculpt this foal, then custom glaze it to a whole new color.  Challenge accepted!  So the first thing I did was drill out the earthenware legs on both sides of the breaks so I could set Kanthal rods into the leg repairs.  I've done leg repairs both ways - with & without rods.  I'm not really sure which method is better, though obviously some pieces are easier to drill out than others.  Material and the thickness of the legs may determine drilling them out to be impractical. 

It is important to note that you can't just use any kind of drill bit.  It must be a diamond coated drill bit both so it doesn't leave metal fragments in or on your ceramic piece that will discolor, but also regular drill bits aren't going to be up to the task of drilling through ceramic.  I prefer to use a hand drill rather than a power tool as you need to go very slowly so not to shatter the thin leg.  The diamond coating also chips & wears off quickly so replace your bits as often as you need.  They are inexpensive because the 'diamond' coating isn't actually diamond of course.

Here you can see the legs of the earthenware ceramic foal have been drilled out to fit in the Kanthal rods.  Now it's time to rough up & score the ceramic so it is as deeply toothy as possible.  Just like slip sticking two pieces of damp clay together, we need the newly added clay to /interlock/ with the already fired clay so it will have a lasting grip even when temperatures or humidity change over time.  Otherwise slick pieces won't hold up and the clay would flake & crack in due time.  The same should be done when joining any two materials really, such as epoxy to plastic or resin because the coeffifiency (expansion & contraction rates) of the two materials may not match. This is what makes it possible to repair even porcelain or fine bone china using a lower fire clay like earthenware!

Again the tools I use, be they files or dremal bits and cutting discs, are all 'diamond' coated.  In the case of cutting deep toothy score marks into the ceramic pieces I wish to join together, I can either do it by hand, or use a power tool.  Unlike drilling down through a thin leg, I don't have to worry about shattering it when I'm just cutting toothy slices through the already fired clay.

Each broken piece is deeply scored using files or cutting discs so that when the new clay is added (first using bisque mender) it will have something to interlock and grip.  The same applies to the Kanthal rods I will cut and insert into the legs.  If they are slick the clay won't necessarily keep a grip on it so I rough up the rod pieces with a file and wire cutters to make it as toothy as possible as well.  You could try using Nichrome wire instead but in my experience the Kanthal works much better and doesn't flake apart like the Nichrome sometimes does.   The two resistance wire types also fire to different Orton cones in the kiln so I prefer the higher firing Kanthal myself.  It is the same wire used in most kilns for kiln furniture, kiln elements, etc.

Once I have 'glued' the leg pieces back together using the rod inserts and bisque mender then I am ready to add regular wet clay over this to build out the leg.  Or you can just use more bisque mender.  As I make my own bisque mender it is cheap and I have ample amounts of it.  With the various additives like gum Arabic to make it stick & dry stronger than regular dry greenware clay, it has some advantages but may be trickier for you to detail once it's dried.

Each leg gets a bit of Kanthal rod inserted and then it is 'glued' on using the bisque mender.  I like to set my pieces upside down so the leg I am working on can be straight up and not angled off to one direction or another.  Use a heater fan or hair drier to help set it up fast.  Don't worry about cracking.  Newly added mender or clay will shrink as it dries, and again when you fire it.  So just fill in the cracks & keep going, don't worry about it.


After drying, the broken legs are then ready to sand & shape up!  At any point I can add regular clay over the repair now if find it at all difficult to work with the bisque mender.  Any cracks are filled and the fine tendons are carefully carved back in.  If you find the legs are too fragile & you keep knocking them off, use bisque mender only.  Sand & shape them, then fire and add details like tendons after the repair has been bisque fired.


Now we have a fully repaired Hagen Renaker 'Sherif' foal all ready to go into the kiln.  I fired this baby slowly to cone 04 as if it were a bisque - simply ignore that it is already glazed.  Firing to cone 04 won't hurt the glaze.  If any cracks appear after the bisque firing just fill them in & sand again.  Complete any detailing using your diamond coated tools if you need to and then you are ready to clear glaze the leg repairs.  Any piece like this that is kiln repaired is no longer technically original finish but it will then be all set for custom glazing!

This concludes PART ONE.  I will continue this blog post in Part 2 - Customizing an Already Glazed Ceramic.

Kiln Repairing Bisques

I do fine art equine sculpture in ceramics.  Finely ball milled earthenware with talc, porcelain, as well as English fine bone china.  I sculpt, mold, cast in studio, but the bulk of my work the past almost 25 years now has been custom glazing bisques sculpted by other artists.  Sometimes I kiln repair very rare, sought after pieces, and sometimes I get permission to resculpt and customize them into whole new collaborations.  It is kind of a unique niche for me that I inhabit, though others also sculpt, cast, or glaze such pieces - they just don't kiln repair or resculpt them past the greenware stage like I do.  So I thought I would post a few photos of some examples & how I do it so you can try it too!


Here is an extremely delicate sculpture called 'Dante' that was sculpted by Sarah Minkiewicz-Breunig & produced in fine art grade earthenware ceramic by Pour Horse Pottery, Joanie Berkowicz.   VERY few of these were produced and most were glazed by Joanie herself, but a few bisques were made available for other glaziers like me to finish.  This one came to me with two broken legs.  A client wanted me to kiln repair & glaze it for her.  Being a very rare and sought after piece, it was well worth the effort to restore it - if I could!   Dante stands about 4 inches tall.

 

 

To kiln repair a bisque (or even an already glazed piece) you need to use a bisque mender.  I used to use a commercially available product made by Coloramics years ago when I first started doing this back around 2006.  I'd been custom glazing ceramic horse pieces for about three years by that point.  Later when I could no longer obtain the bisque mender I had to learn to make my own because I could not find another product that worked nearly so well or cracked so little.  If you attempt this I suggest you try a commercially available bisque mender to start or ask me for my recipe if you want to try making your own!


First I rough up and 'score' the bisque just like piecing together slabs of wet clay.  I make it as toothy and grabby as possible so that the clay mender can interlock with the already fired ceramic.  I use a roto tool with diamond cutting discs, or you can use a diamond coated file to cut into the bisque by hand.  It doesn't matter if it's earthenware, porcelain, stoneware, or fine bone china.  Just be sure to wear suitable protection for your eyes & respiration.  I use a damp paper towel underneath the work so any dust settles onto it.  A damp sponge to wipe it up also works, you just don't want to breath the ceramic dust.


If the legs are thick enough I may drill them out and set in roughened kiln rods (Kanthal) before layering with bisque mender & clay.  I'll make a whole other post about that using an already glazed ceramic for that example.  Dante's legs were just too thin to benefit as drilling them out would likely have shattered them.

 

 

Making the ceramic as toothy and grippy as possible is the MOST important step, else the added clay may flake and pop off later.  I then 'glued' each piece back into place using the bisque mender and layered clay right over it.  Once it was at least leather hard or dry I could very CAREFULLY clean it up.  Very fragile and hard not to knock right back off!  If you knock off the leg just be patient and do it again.  I've used painter's tape to help support & turn the piece upside down so the leg can dry a upright as possible.

 


 

I had to sand & redetail the tendons on each leg before firing it to cone 04.  The toothy scoring allows the newly added clay to grip & interlock even if the co-efficiency rates between the materials are not a match, such as using earthenware to repair porcelain.  Some people use actual porcelain bisque mender to repair porcelain but taking an already fired bisque all the way back up to those temperatures has it's own issues when you no longer have the original props that were fired with it.  


When the newly added clay dries it cracks - so be patient and just fill in the cracks & smooth it again.  Bisque firing the ware will also make it shrink and crack AGAIN.  Don't freak out over it.  Just fill in the cracks with more bisque mender, sand & clean up the details, and bisque fire a second time.  Yes, it takes patience and tenacity.  If you didn't do a great job before it was bisque fired you can /still/ refine, sand, file, roto tool carve, add more bisque mender until you get it just right.  Do not be discouraged.  Just keep going!  This has taken me practice so trust me when I say my first attempts were imperfect.

 



Once it is all finally together and as good as you can get it, bisque fire him to cone 04.  Typically I have to fill in tiny cracks and fire twice.  Joanie has my profoundest respect that she could mold, cast, and glaze these at Pour Horse Pottery.

 

Here is the SAME Dante bisque that I posted before with the two broken legs - now all repaired in the kiln.  From here I could make him a custom base because he is a tippy, fragile little sculpture.  After under glazing & clear glazing I then proceeded to overglazing him with china paints and enamels.  My client couldn't have been more thrilled! 

 

 

I have to date kiln repaired three of this rare sculpture.  I consider myself highly fortunate with my progress, trial & error to learn how to restore these amazing pieces.  Over the past 20+ years I have been doing this kind of kiln work, I know of only one piece that cracked & flaked off a thin area later that wasn't scored & made toothy enough.  I think that's a pretty good track record BUT test, test, test so your clients don't get stuck with your screwups self destructing later!

 

You can see all three (soon to be four) Dantes I have custom glazed on my website under custom glazed ceramics. 

How I Paint Micro Mini Horse Sculpture

I thought I would share a bit about how I paint micro mini equine sculpture - the basics of how I mask a pattern and then rough it out using an etching technique is the same for me whether it's a micro or a larger piece, cold painted or custom glazed.  Over which I then add layers of paint using cut down detail brushes to refine and soften details.  The etching left by itself is, in my opinion, too coarse.  Especially on micro minis!  This post is not intended to take the place of an actual 'hands on' workshop where I can help you every step of the way, but is a brief introduction.  There is no right or wrong way to paint micro minis, this is just how I do them myself.

The first step is priming the micro to remove any seams or 3D printing marks, nubs, divots, print lines, etc using fine sand paper or steel wool.  If pewter I buff them well with 0000 steel wool to remove any mold release, oxidation, and to add micro scratches to the surface to better hold painted layers.  Then I mount them onto an easy to hold thick rod using double sided foam tape and airbrush prime my micros with a layer of smooth white acrylic.  That layer needs to cure over night before proceeding.  Any white markings are masked using liquid latex which I remove after I have airbrushed on my basic color.  This is a micro mini Stormwatch sculpted by Sarah Minkiewicz-Breunig and 3D printed in resin, just begun as a dark bay sabino.  Masking has been removed but not yet cleaned up.

The next phase is to rough in the pattern using an fine tipped craft knife.  I am very careful to try not to cut through the white paint layer and only remove the colored layer as much as possible.  If I do accidentally cut through the white layer I just touch it up with carefully with white paint later.  In the video below I have roughed in the appaloosa pattern on a 'Maelzela' micro sculpted by Maggie Bennett and cast in pewter rather than resin.  You may open the video full screen if you wish to view it larger.

Etching alone will be too coarse and rough, especially for a micro.  But with any size piece once I have laid in the hair pattern and detailed it as far as I can reasonably go, I will then continue with additional layers over top that I paint very carefully.  For micros I cut down used up old detail brushes to just a few short hairs for ultra fine detailing and I use a magnifying lamp to see up close.  I also use my phone to zoom way in and see if there are areas I still need to refine and clean up better on later layers.  Below is the same micro mini Stormwatch 3D printed resin showing his other side with thin paint being added to soften and expand his white areas further for roaning effects.  Over this I also add tiny darker color spotting for sabino lacing and add pastel or oils to start pushing his base color richer.  If I use any colored pencil I use low wax brands and make sure they are well sealed with varnish so it can't rub off later with handling.

With patience, magnification, and many layers, details can be refined.  Typically I don't paint more than one micro mini in a given month.  While the actual work can be completed within about a week or less my poor eyes and back require many breaks to work on larger pieces.  Layering up and refining the details over and over and OVER again takes persistence and a refusal to stop until I am satisfied with every aspect, however long it takes!  I will use my magnifying lamp and my phone to zoom in and check every little bit including the tedious painting of the eyes!

Finally when you are completely finished make sure you seal your work so it is protected from damage and is easy to clean.  I strongly suggest that if you invest in collecting micro minis of any kind that you either always wear clean white museum gloves when handling them, or wash your hands EVERY time before you pick them up.  Otherwise skin oils and dirt will quickly make a stunning and expensive paintjob look dirty and drab.  If sealed properly and handled with care, such pieces can last a life time and more!  I make mine durable enough to be gently washed with soap and water if they get dingy over time.

Here the appaloosa 'Maelzela' has been completed, sealed with matte varnish with glossed eyes and hooves.  I have decorated her custom sculpted base as a custom order for a client.  Photographing such pieces can be quite a challenge in itself, and then packing them for shipping!  Some of these micro minis only stand a little over one inch tall, or less, and can be very fragile.  Depending on what they are made of I either double box them or cut custom foam just like I do when I ship fragile ceramics.  Enjoy and I hope you find this brief, free tutorial inspiring on how I paint micro mini equine sculpture.

 

 

Watch Your Firing Times...

A while back I mentioned on my Workshops Facebook group that my large Skutt kiln cost a small fortune in electricity to fire and that a newer kiln wouldn't have that issue.  Which turns out to be true - in a simplified way.   A long firing using my Skutt after 20 years was taking too long and eating a lot of power.   It might run me $50 in electricity to do a single long, slow firing and that's nuts.  But for a while I had used this kiln so little until the past year that I forgot how long the firing schedule should have been.

While firing the Cybis 'Nashua' I've been working on for a while, one evening my kiln finally threw an error code and aborted the firing.  Thankfully my client's Cybis wasn't ruined.  It merely didn't fire up to temperature.  Either one of my kiln elements had blown or my thermocouple had gone bad.  Testing was in order.  A simple multimeter (while the power was disconnected) showed me a LOT of resistance in the elements that still worked.  I then ordered new elements for my Skutt and they arrived yesterday!  Mind you, BOTH of my kilns have been used much of the past 20 YEARS and NEVER had anything replaced on them until last year.   My Skutt especially still looks brand new.  My Olympic suddenly blew a relay and that was a wake up call for me!  Now this.

Needless to say I should have replaced the relays and elements YEARS ago.  Expensive as they are I've surely wasted several times the cost in electricity in just the past few years due to having worn out elements and not realized it.   All my firings have continued to go just fine - I just wasn't keeping a log of how long it took for those firings.  If I had been I'd have seen that my firing times were getting longer and longer over the years.  It did that so slowly I didn't even notice.  I barely even use this large Skutt kiln compared to my little Olympic Doll E so why would I have caught that?

 

As I am fond of saying, 'No matter how much you think you know about anything, there is ALWAYS more to learn!'  Ceramics is definitely no exception to that rule.  So guess what I am doing today?   Replacing all four elements in my Skutt.  I've got this!  There's a YouTube video for almost anything out there...

 


What is Underglazing of Ceramics?

 

The first ceramics based workshop I have in mind to host this year will be an underglazing workshop, tentatively slated for October 2023 followed by an overglazing workshop probably the following spring around April or May.  Keep an eye on my 'Events' menu for workshop dates or join my email list.

What is underglazing? This is a process where pigments, mixed with clay or other silica based ingredients that will fuse when fired in a kiln, are applied to a ceramic bisque to color it. Underglaze by itself can be fragile, especially when raw and unfired. It is usually covered over with a clear glaze to protect it and bring out the richness of the pigments. This is a decorating technique used by Hagen Renaker and many other animal ceramics manufacturers the world over. It is more durable than over glazing, generally less toxic, and requires a higher heat to set, usually the same temperature low fired ceramics are bisque fired at - typically Orton cone 04. Many underglazes can be fired at much higher temperatures and will eventually, when hot enough, melt and become glossy glazes in their own right. 

I like to use underglazes because you have very precise control of the finest of details. Unlike overglazes, underglazes DO NOT MOVE around when fired. Overglazes to some degree will melt, blur or bloom softly and it is very difficult to get extremely precise, fine layers of super sharp, crisp detail - especially with repeat firings.  Overglazes float on top of the clear glaze or sink into it unless applied directly to non-porous bisque.  Don't get me wrong - I use over glazes as well and love their richer colors.   I think together, using both under glazing with over glazing allows me the greatest possible flexibility to achieve my desired goals.  More about the benefits of over glazes in a future article! 

But underglazes do not necessarily retain the super saturated colors that overglazes give to finished pieces. They are less 'what you see is what you get' than over glazes.  Underglazes as a rule however are usually less toxic than most over glazes and thus safer for airbrushing.  You still want to wear suitable respiratory protection due to the silica content.  More about that in an upcoming post.

Underglazes can be masked, etched with individual hair details, layered, and even have very crisp fine hair by hair painted details. I prefer underglazes when I want to set precise white markings, white hair ticking, fine edges to pinto or appaloosa patterns, and even for some hand painted detail work.

The primary drawback to underglazes is that the colors you apply don't look exactly like what you'll get on the finished piece. Colors are paler and sort of washed out until the clear glaze is fired over them to bring out their true hues. Every kind of clear glaze will effect the final color differently - different levels of gloss or matte, or even changing from one brand to another can affect the final color you will get after firing.

Also, the oxygen level in the kiln during firing, as well as the exact temperatures at the location of the fired piece, can cause the underglaze colors to shift hue. So the results can sometimes be unexpected. Testing, trial and error, and note taking are encouraged with using underglazing. When you have access to a kiln it is standard procedure for ceramists to do many test tiles with underglazes with both hand painted and airbrushed layers, paired up with various clear glazes to see how they turn out under your particular firing conditions. 

Do you need better reds in your browns that keep firing out too dull or even greenish?  Place those pieces higher on shelves in the kiln, pull out your peep holes and maybe even prop your kiln lid ever so slightly open for more oxygen - but beware, it'll take longer to fire that load and cost more electricity to do so.  The same /can/ be true for some over glazes that also require more oxygen when firing.  This is also true of blacks - adding some red or red brown can help you not to have cold or greenish hues in firing.  Remember I mentioned trial and error and note taking? ;)

For our purposes we'll start with masking a bisque and then airbrushing underglaze over the piece. This is why you will need to acquire and practice with using an airbrush and learn the safety precautions so not to breathe in the silica dust it generates. Underglazes can be applied in layers using a brush by hand or a sponge but will not give smooth coats without texture or streaking. There are both opaque and transparent forms of underglazes.  I mostly use opaque underglazes but transparent ones do have their uses in adding additional layering.

Below is an example of a bone china bisque with raw, unfired black underglaze with detailing and clean up shown in progress. Airbrushed over the piece it can then be carefully detailed (remember it is very fragile and easy to scratch or scuff!) and once detailed, it is fired to set the first layer. It is not unusual for me to fire pieces several times before I apply the clear glaze.  It is also not unusual for me to have to trim my fingernails before working on a piece.  I am all the time scratching my underglazes where I don't mean to, or gouging my freshly slip cast greenware.   The things we do for ceramics!


 

Articles and photos are copyrighted and may not be reproduced without permission of the author.

Custom Glazing 'Horse Shaped Objects' - Basic Introduction

 

I started a group on Facebook for my upcoming custom glazing workshops.  It occurred to me that since I'm not yet diving into a Patreon page or similar setup, I may as well make all of my basic starter information posts completely public here on my blog and not just restricted to a private group on Facebook.  If these posts are helpful to get others set up and working in ceramics, producing their own sculpture, and trying various forms of custom glazing (for horse shaped objects or otherwise) then I'm glad if these posts might be helpful to you.  Mostly however they are aimed at those involved in the Model Horse Hobby or fine art equine sculpture, but can equally apply to any animal ceramics.

What is a ceramic bisque? The word "ceramics" comes from the Greek word keramikos meaning "of pottery" or "for pottery". The term "bisque" is of French origin and actually means 'twice baked' which is interesting since in ceramics it refers to raw 'greenware' clay that has been fired for the first time to partially or fully 'vitrify' the clay particles, fusing them together enough so that the clay will no longer turn back into mud when wet.

In our case, 'bisque' is used to generally refer to once fired clay that is it's natural, raw color state and undecorated. That could be white, tan, brown, grey, black, etc depending on the clay used and also may included tinted slips.   Some also use it to refer to decorated pieces that lack actual silica based glassy glazes, such as bisques that have been china painted and refired again, but don't actually have higher fired glazes applied.  There is a lack of uniformity in the use of the term so you may run into some confusion.  For my articles we will be using the term to indicate a completely undecorated piece of clay that has been fired at least once or more but still has the original clay color.  This is the most common use of the term by most ceramists, if not also collectors.

By contrast, another term to make yourself familiar with is 'white ware'. This generally refers to any bisque that is white and has been fired with a clear glaze, glossy or matte, but is otherwise completely undecorated with color.  For the purposes of under glazing we will use true 'bisques' only.  However, for over glazes we usually apply these over a piece that has already been glaze fired - white ware or colored but in some cases over glazes can also be applied directly to bisques.  Usually non-porous bisques such as porcelain or bone china.   In my case, I use both under glaze and over glaze techniques together at various stages.

To get everyone started in learning the terminology, I highly recommend readers of this blog interested in learning custom glazing to book mark and start reading the https://digitalfire.com/ website's glossary of terms.   There is a wealth of information there about the history of ceramics and all of the many terms we'll be using to discuss the materials and processes I'll be covering in my ceramics based workshops and blog posts.  Or you may look up individual, unfamiliar words in general internet searches.  The more you know the better you will understand these posts as I delve into the art of fine equine custom ceramics.  There are also some very helpful ceramics forums out there to give you help along the way and aid with trouble shooting such as Ceramics Arts Network and their hugely helpful forum, Ceramics Arts Daily.

Below is a sample unglazed earthenware bisque 'Okie Rio' shown here with a custom mane added by myself, ready to start under glazing.  This beautiful weanling stock horse was sculpted by the well known Carol Williams of Rio Rondo and produced both glazed and in bisque by Pour Horse Pottery.   I'll post more about bisques soon, what you will need, where to find them, and varieties and sizes that would be ideal to locate for my workshops or to practice on at home when you first get started on your own.   Save any expensive, rare pieces for later once you master a few skills!

All blog posts and images are copyrighted and may not be reproduced without written permission.

 

Cybis 'Nashua' Porcelain Race Horse Customization

A while back a client asked me if I could try reworking a great big Cybis thoroughbred porcelain named 'Nashua'.  Now he wasn't an undecorated white bisque but an already colored piece epoxied to a huge base.  On the base he measures about 13 or 14 inches tall and with his original wooden plinth beneath it (now missing) he would have topped 16 inches tall.  Anyway, this client owns more than one of this sculpture and choose to send me the flawed one to custom glaze.

Here he is in his original bay color and on his original rectangular base sitting down in the bottom of my big kiln.  Nashua was sculpted by J N Slick and supposedly released in a 500 piece porcelain edition in 1971, priced at $2000.  According to the Cybis Archive the edition was aborted and only 100 were produced even though higher numbered pieces exist.

Nashua was sent to me because he had a rough finish that captured dust and his owner was not able to get or keep him clean.  I offered to fire him clean in my kiln at a fairly low temperature to burn off the accumulated dust.  To our surprise it turns out that he was fixed to his original base with some kind of epoxy which also burned away in my kiln.  Once off of his base I saw that his feet were wonky and he did not stand flat and his legs were subtly bent.  He also leaned precariously without his base to keep him straight upright.  My client asked me if I might be willing to reglaze him to another color and sculpt him a new base that wasn't so big and clunky.  I said I could try, but reglazing a piece can be tricky.  One never knows if my glazing will be compatible with the co-efficiency of the original porcelain, even though I do my glaze firings at much lower than the original bisque firing.  I also do not know if he was clear glazed before coloring or if it was applied directly to the raw bisque - probably the latter.

Here is the Nashua removed from his base.  He had a metal halter ring made of brass that I removed before firing that I will replace once he's finished.  Now he's all clean and pretty but he won't stand on his own and firing him clean will do nothing to keep him from turning back to a muddy grey over time.  Not unless his owner closes him up into a case to keep dust off or have him reglazed smoother. 

As he couldn't stand without the base, we sadly can't have him free standing without one.  I had to add balls of sticky putty under both of his hooves on one side to keep him from falling over.  I might have removed material from two hooves and added more to the other two but it was just too much difference and his hooves would have been too obviously strange sizes, alas.

This boy had some notable seam lines, rough finish in places, and a pretty drab mane and tail with rough patches.  Her other Cybis 'Nashua' she kept is a much nicer copy.  I proposed slightly resculpting his mane and tail, removing those seam lines, and adding a bit more expression to his eyes.  She said go for it!

Here our boy is getting his new base sculpted in non-hardening oil clay.  Once I had it roughed out how I wanted it, I then made a plaster mold.  The plaster mold, once cured, was then used to slip case Nashua a new base.  His new base then could be fired and glazed right a long with him in the kiln.  Shrinkage could be compensated for after the initil bisque fire.  Here's a shot of the freshly made plaster mold.  This could be done as a one or two piece mold depending on  how I wanted it to cast.

To demonstrate the size of this piece, here I have Nashua standing next to a more 'traditional' scale ceramic.  The other horse is a English fine bone china 'Precosia' produced by Horsing Around of England and sculpted by Brigitte Eberl of Germay.  She was in progress getting made into a boy with a new mane and tail just like the Nashua!  You can see on him the freshly added clayed up mane and tail.  Resculpting work is a lot more complicated than just adding wet clay, which will shrink, crack, and flake off.  So I have been working for about 20 years now to perfect this technique using a custom 'bisque mender'.  As far as I know I'm the only person in the world who does it.  Yet pieces I did back in the early 2000's are still doing great more than twenty years later! 

Note that I am adding specialty chemicals to the original porcelain that has been gouged and roughed up to receive the earthenware bisque mender and clay.  Once dried, one has to painstakingly fill in cracks several times before and after firing to make certain the material will hold & grip firmly.  I can't add back high fired materials like porcelain because that must be fired up to a high enough temperature to vitrify, which means I would have to prop pieces all over again so they don't become jelly like and sag/warp.  I could try to do so but I do not know what this porcelain claybody is actually composed and what cone it was originally fired to, and any supports I added would be greenware and thus shrink too much. Using a lower fired ceramic media in the range of the custom glazing works so much better as long as I have deeply scored the porcelain I am attaching it to for a mechanical grip that won't crack or flake off with any difference in co-efficiency (expansion & contraction) of the two materials with temperature changes.

Once I get the mane, tail and base dried, then I use opaque white under glaze to 'white' out the bay body.  This helps me see rough patches, divots, or cracks I have missed and need to work on before he's fired again.  Seams still showing through under his jaw or along his belly, further detailing to do in cleaning up his new mane, smoothing roughness over his body, etc.  Then he'll be ready for me to begin custom glazing to his new color!  The white layer will likely sink into the original bay coat and mostly be lost but I won't know until I fire him.   There is always the risk that this particular porcelain that Cybis used may not be a good fit with my cone 06 glazes, but I am keeping some leaded clear glaze on hand in case there is a co-efficiency issue.  I do not want to risk crazing or dunting when he is completed.

Now he's ready to go back into my kiln to bisque fire at cone 04 to set up his greenware clay parts and first under glaze layer.  The underglaze layers and clear glaze over it later will help a lot to smooth out his rough texture.   Stay tuned for Part 2 of the Nashua custom glazing adventure!  After he is fired and passes close inspection, Nashua will be ready to start masking white markings and layering up under glaze colors for his new coat color!  I do enjoy an unusual custom order request.

Turns out that the 'whiting' out effect didn't actually work over the kind of coloring he already had but it still served it's purpose to help me see rough areas that still needed smoothing.  It was merely absorbed into the original color so I had to work with that.  After speaking with my client she changed her mind and was willing to accept a dark dappled bay instead of a lighter golden bay.  Whew!  There are limits of what I can do when attempting to reglaze an already glazed ceramic.

It took me quite a while and a LOT of firings using both china paints & enamels but eventually he was completed to this lovely dark dappled bay!  After all firing in the kiln was completed I added the brass ring back to his halter.  His owner is thrilled with him!  It was very challenging work!  I hope you enjoyed this blog post and apologies it took me so long to add the conclusion.  Enjoy and be inspired to try your own thing - don't be afraid!